The influence of cure characteristics and crosslink density of virgin acrylonitrile butadiene rubber/recycled acrylonitrile butadiene rubber (vNBR/rNBR) blends
Date
2014Author
Muhammad Ridhwan, Jamalul Nasir
Nik Noriman, Zulkepli, Dr.
Hanafi, Ismail, Prof.
Mohd Mustafa Al Bakri, Abdullah
Rosniza, Hamzah
Metadata
Show full item recordAbstract
Cure characteristics and crosslink density of virgin acrylonitrile butadiene rubber/recycled acrylonitrile butadiene rubber (vNBR/rNBR) blends were studied. Three different size ranges of rNBR particles, i.e., 150 - 350 μm, 2.0-15.0 mm, and 5-10 cm were used in this study. The vNBR/rNBR blends with blend ratios of 95/5, 85/15, 75/25, 65/35, and 50/50 were prepared using a two roll-mill at room temperature. The characterization results of the blends show that scorch time, t2, of the vNBR/rNBR blends decreased with increased rNBR content as well as decreasing sizes of rNBR particles while cure time, t90 of the vNBR/rNBR blends increase with increased rNBR content as well as increasing sizes of rNBR particles. Among all blend ratios, the vNBR/rNBR blends with smallest size of rNBR particles exhibit lowest minimum torque (ML) compared with the bigger particle sizes of it in vNBR/rNBR blends which resulted in more efficient processing. The maximum torque (MH) of all vNBR/rNBR blends shows the inclining trend with increased rNBR. The cross-linking density of vNBR/rNBR blends also show an increasing trend with increasing rNBR content.