Effect of Solids-To-Liquids, Na2SiO3-To-NaOH and Curing Temperature on the Palm Oil Boiler Ash (Si + Ca) Geopolymerisation System
View/ Open
Date
2015Author
Zarina, Yahya
Mohd Mustafa Al Bakri, Abdullah
Kamarudin, Hussin
Khairul Nizar, Ismail
Rafiza, Abd Razak
Sandu, Andrei Victor
Metadata
Show full item recordAbstract
This paper investigates the effect of the solids-to-liquids (S/L) and Na2SiO3/NaOH ratios on the production of palm oil boiler ash (POBA) based geopolymer. Sodium silicate and sodium hydroxide (NaOH) solution were used as alkaline activator with a NaOH concentration of 14 M. The geopolymer samples were prepared with different S/L ratios (0.5, 1.0, 1.25, 1.5, and 1.75) and Na2SiO3/NaOH ratios (0.5, 1.0, 1.5, 2.0, 2.5, and 3.0). The main evaluation techniques in this study were compressive strength, X-Ray Diffraction (XRD), Fourier Transform Infrared Spectroscopy (FTIR), and Scanning Electron Microscope (SEM). The results showed that the maximum compressive strength (11.9 MPa) was obtained at a S/L ratio and Na2SiO3/NaOH ratio of 1.5 and 2.5 at seven days of testing.