    Yttria stabilized zirconia formed by micro ceramic injection molding: Rheological properties and debinding effects on the sintered part

    Thumbnail
    View/Open
    Yttria stabilized zirconia formed by micro ceramic injection molding - Rheological properties and debindingeffects on the sintered part.pdf (26.13Kb)
    Date
    2013-04
    Author
    Farhana, Mohd Foudzi
    Norhamidi, Muhamad
    Abu Bakar, Sulong
    Hafizawati, Zakaria
    Metadata
    Show full item record
    Abstract
    Micro Ceramic Injection Molding (μCIM) is a near net-shape process to produce smaller and intricate parts at a competitive cost. The application of nano-sized ceramic powder in μCIM has the advantages of fine grain size growth and good surface finish. However, the nano size effect causes agglomeration and low powder loadings, which result in defects during the μCIM process and in the sintered components. This study extensively investigated the debinding and sintering of yttria-stabilized zirconia (YSZ), as well as its rheological properties, using polypropylene (PP) as the primary binder and palm stearin as the secondary binder. 50 nm Yttria stabilized zirconia (YSZ) powders were mixed with palm stearin and PP at a powder loading of 37-43 vol%. The results of rheological studies showed that the feedstock had a dilatant flow characteristic and a viscosity of around 10-40 Pa s. Feedstock with 38 vol% powder loading had the lowest activation energy of 9.48 kJ/mol. The green part of the injected feedstock had flexural strength ranging from 13 to16 MPa, within which the feedstock with 43 vol% powder loading had the highest green density. Solvent debinding was carried out at three temperatures (50, 60, and 70 °C) using heptane. A large porous region was clearly identified at 70 °C compared with 50 °C. A debinding split furnace with argon gas was used to remove PP at 450 °C for 4 h. The debound samples did not shrink when 94%-98% of the binder system was removed. All debound samples sintered at 1350 °C and 41 vol% had the highest mechanical properties with hardness of 900 HV and a flexural strength of 400 MPa.
    URI
    http://www.sciencedirect.com/science/article/pii/S0272884212008838#
    http://dspace.unimap.edu.my/123456789/27308
    Collections
    • School of Mechatronic Engineering (Articles) [319]
    • Hafizawati Zakaria [11]

    Atmire NV

    Perpustakaan Tuanku Syed Faizuddin Putra (PTSFP) | Send Feedback
     

     

    Browse

    All of UniMAP Library Digital RepositoryCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    Atmire NV

    Perpustakaan Tuanku Syed Faizuddin Putra (PTSFP) | Send Feedback