This paper studies the finding of strength and water absorption of geopolymer bricks using bottom ash and fly ash as a geopolymer raw material for non-loading application with minimum strength. The study has been conducted to produce bottom ash and fly ash geopolymer bricks by varying the ratio of fly ash-to-bottom ash, solid-to-liquid and sodium silicate (Na2SiO3)-to-sodium hydroxide (NaOH) in the mixing process. The compressive strength range between 3.8-4.5 MPa was obtained due to the minimum strength of non-loading application with 70°C curing temperature within 24 hours at 7 days of ageing. The optimum ratio selected of bottom ash-to-fly ash, solid-to-liquid and Na2SiO3-to-NaOH are 1:2, 2.0 and 4.0 respectively. The water absorption result is closely related to the amount of bottom ash used in the mix design.