dc.contributor.author | Nik Zakaria, Nik Yahya | |
dc.contributor.author | Nik Noriman, Zulkepli, Dr. | |
dc.contributor.author | Mohd Arif Anuar, Mohd Salleh | |
dc.contributor.author | Hanafi, Ismail, Prof. | |
dc.contributor.author | Ragunathan, Santiagoo | |
dc.date.accessioned | 2014-04-10T07:24:24Z | |
dc.date.available | 2014-04-10T07:24:24Z | |
dc.date.issued | 2014 | |
dc.identifier.citation | Key Engineering Materials, vol.594-595, 2014, pages 634-638 | en_US |
dc.identifier.issn | 1662-9795 | |
dc.identifier.uri | http://dspace.unimap.edu.my:80/dspace/handle/123456789/33591 | |
dc.description | Link to publisher's homepage at http://www.ttp.net/ | en_US |
dc.description.abstract | Curing characteristics and swelling behavior of natural rubber/styrene butadiene rubber/recycled nitrile glove (NR/SBR/rNBRg) blends were investigated. Eleven composition ratio; 50/50/0, 50/40/10, 50/30/20, 50/20/30, 50/10/40, 50/0/50, 40/50/10, 30/50/20, 20/50/30, 10/50/40, and 0/50/50 of SMRL/SBR/rNBRg with the size of rNBRg ; 2.5 3.0 cm2 were prepared by using two roll mill at room temperature. Cure characteristics such as scorch time,t2, cure time,t90, minimum torque, ML, maximum torque, MH, and swelling behavior of SMRL/SBR/rNBRg ternary blends were examined. Results indicated that the scorch time and maximum torque of the NR/SBR/rNBRg blends decreased with increasing rNBRg content. The minimum torque of the blends increased as rNBRg content increased. The cure time of NR/SBR/rNBRg blends show a unique trend, which are depending on the domain rubber content. The increment in rNBRg content decreased the crosslink density of NR/SBR/rNBRg blends. | en_US |
dc.language.iso | en | en_US |
dc.publisher | Trans Tech Publications | en_US |
dc.subject | Crosslink density | en_US |
dc.subject | Curing characteristic | en_US |
dc.subject | Natural rubber (NR) | en_US |
dc.subject | Recycled nitrile glove (rNBRg) | en_US |
dc.subject | Styrene butadiene rubber (SBR) | en_US |
dc.subject | Ternary blend | en_US |
dc.title | Natural rubber/styrene butadiene rubber/recycled nitrile glove (NR/SBR/rNBRg) ternary blend: Curing characteristics and swelling test | en_US |
dc.type | Article | en_US |
dc.identifier.url | http://www.scientific.net/KEM.594-595.634 | |
dc.identifier.doi | 10.4028/www.scientific.net/KEM.594-595.634 | |
dc.contributor.url | nikzakariany90@gmail.com | en_US |
dc.contributor.url | niknoriman@unimap.edu.my | en_US |
dc.contributor.url | hanafi@eng.usm.my | en_US |
dc.contributor.url | arifanuar@unimap.edu.my | en_US |
dc.contributor.url | raguna@unimap.edu.my | en_US |