Show simple item record

dc.contributor.authorDewi Suriyani, Che Halin
dc.contributor.authorMohd Mustafa Al Bakri, Abdullah
dc.contributor.authorNorsuria, Mahmed
dc.contributor.authorS N A, Abdul Malek
dc.contributor.authorVizureanu, P
dc.contributor.author‪Ayu Wazira, Azhari
dc.contributorCenter of Excellence Geopolymer & Green Technology (CEGeoGTech), School of Materials Engineering, Universiti Malaysia Perlis, (UniMAP)en_US
dc.contributorFaculty of Engineering Technology, Universiti Malaysia Perlis, (UniMAP)en_US
dc.contributorSchool of Environmental Engineering, Universiti Malaysia Perlis, (UniMAP)en_US
dc.contributorFaculty of Materials Science and Engineering, Gheorghe Asachi Technical University of Iasien_US
dc.date2022
dc.date.accessioned2022-03-07T06:41:41Z
dc.date.available2022-03-07T06:41:41Z
dc.date.issued2017-06
dc.identifier.citationIOP Conference Services: Material Sciences Engineering, vol.209, 2017, 8 pagesen_US
dc.identifier.issn1757-899x (online)
dc.identifier.urihttp://dspace.unimap.edu.my:80/xmlui/handle/123456789/74583
dc.descriptionLink to publisher's homepage at https://iopscience.iop.org/en_US
dc.description.abstractTiO₂/SiO₂ thin films were prepared by sol-gel spin coating method. Structural, surface morphology and optical properties were investigated for different annealing temperatures at 300°C, 400°C and 500°C. X-ray diffraction pattern show that brookite TiO₂ crystalline phase with SiO₂ phase presence at 300°C. At higher temperatures of 400-500°C, the only phase presence was brookite. The surface morphology of film was characterized by scanning electron microscopy (SEM). The films annealed at 300°C shows an agglomeration of small flaky with crack free. When the temperature of annealing increase to 400-500°C, the films with large flaky and large cracks film were formed which was due to surface tension between the film and the air during the drying process. The UV-Vis spectroscopy shows that the film exhibits a low transmittance around 30% which was due to the substrate is inhomogeneously covered by the films. In order to improve the coverage of the film on the substrate, it has to repeatable the spin coating to ensure the substrate is fully covered by the films.en_US
dc.language.isoenen_US
dc.publisherIOP Publishing Ltden_US
dc.relation.ispartofseriesInternational Conference on Innovative Research (ICIR Euroinvent 2017);
dc.subject.otherThin filmsen_US
dc.subject.otherTiO₂/SiO₂ thin filmsen_US
dc.titleSynthesis and characterization of TiO₂/SiO₂ thin film via SolGel methoden_US
dc.typeArticleen_US
dc.identifier.doihttps://doi.org/10.1088/1757-899x/209/1/012002